Filler/Reinforcement: Unspecified Nano
Additive: Heat Stabilizer
Features: Good Impact Resistance; Heat Stabilized
Uses: Electrical/Electronic Applications; Tubing; Wire & Cable Applications
RoSH Compliance: RoSH Compliant
Appearance: Natural Color
Forms: Granules
Processing Method: Extrusion
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide