Description: TWP61 is a complex-carbide flux cored wire electrode used to protect equipment and parts from heavy wear in extreme temperatures. TWP61 has a unique composition that forms a tight crystalline matrix, and is able to deter heavy wear in temperatures up to 842oF (450oC). Key Performance Characteristics: Heavy abrasion resistance, High heat resistance, Tight crystalline matrix,Good corrosion resistance Applications: TWP61 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recommended deposit thickness of TWP61 3/8” (9.53mm) in 2 - 3 layers. TWP61 is used for the installation of T157 wear plate and parts, as well as for hot wear applications such as burner tips, classifier cones and smokestacks. Information provided by Trimay® |