MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Chromium-molybdenum-tungsten-vanadium alloyed PM steel

Vanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications where wear resistance above that of an ORVAR 2M / AISI H13 is required. This material is available in limited sizes.

Vanadis 23 is characterized by:

  • High wear resistance (abrasive profile)
  • High compressive strength
  • Very good through-hardening properties
  • Good toughness
  • Very good dimensional stability on heat treatment
  • Very good temper resistance
Applications: Uddeholm Vanadis 23 is especially suitable for blanking and forming of thinner work materials where a mixed (abrasive–adhesive) or abrasive type of wear is encountered and where the risk for plastic deformation of the working surfaces of the tool is high, e.g.:Blanking of medium to high carbon steel
  • Blanking of harder materials such as hardened or cold-rolled strip steel
  • Plastics mould tooling subjected to abrasive wear condition
  • Plastics processing parts, e.g. feed screws, barrel liners, nozzles, screw tips, non-return check ring valves, pellitizer blades, granulator knives

  • Vendors:
    Available Properties
    • Density, hardened and tempered
    • Density, hardened and tempered
    • Density, hardened and tempered
    • Hardness, Brinell, Soft annealed (Delivery condition)
    • Hardness, Rockwell C, Tempering: 3 x 1 h at 1040°F
    • Modulus of Elasticity, (hardened and tempered)
    • Modulus of Elasticity, hardened and tempered
    • Modulus of Elasticity, hardened and tempered
    • Flexural Strength, Four-point bend, (Fracture) @58HRC, Tempering: 3 x 1 h at 1040°F
    • Flexural Strength, Four-point bend, (Fracture) @62HRC, Tempering: 3 x 1 h at 1040°F
    • Flexural Yield Strength, Four-point bend, @58HRC, Tempering: 3 x 1 h at 1040°F
    • Flexural Yield Strength, Four-point bend, @64HRC, Tempering: 3 x 1 h at 1040°F
    • Impact Test, unnotched; Tempering: 3 x 1 h at 1040°F
    • CTE, linear, hardened and tempered
    • CTE, linear, hardened and tempered
    • Specific Heat Capacity, hardened and tempered
    • Specific Heat Capacity, hardened and tempered
    • Specific Heat Capacity, hardened and tempered
    • Thermal Conductivity, hardened and tempered
    • Thermal Conductivity, hardened and tempered
    • Thermal Conductivity, hardened and tempered
    • Shrinkage, Austenitizing and tempering
    • Carbon, C
    • Chromium, Cr
    • Iron, Fe, As Balance
    • Molybdenum, Mo
    • Tungsten, W
    • Vanadium, V
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    New MatWeb Services
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.