MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lanxess LEWATIT® SM 600 KR Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® SM 600 KR is a ready-to-use mixed bed resin comprising strongly acidic gel-type cation and strongly basic (type I) gel-type anion exchange resin in fully regenerated form (min. 99% H/95% OH). Lewatit SM 600 KR is a 1:1 stoichiometric mixture (other mix ratio available on request), premium grade and purified (extremely low content of desorbable chloride ions and no organically bound chlorine) to meet nuclear industry specifications. Lewatit nuclear resins (Lewatit KR) are noted for their outstanding mechanical and chemical stability as well as their high osmotic stability. Because of their excellent hydrodynamic properties, Lewatit KR resins allow particularly high flow rates. The narrow particle size distribution and very low fines content of max. 0.1% (<3.15mm) result in particularly low pressure losses compared with standard resins. Used in radioactive water circuits, they provide a number of special tasks and guarantee a water quality that fully complies with the requirements of the nuclear power industry. Lewatit SM 600 KR is particularly suitable for the:
  • polishing in the primary and secondary sections as a mixed bed component
  • decontamination of circuits in nuclear reactor plants
  • treatment of primary coolant e.g. in pressure water reactors
  • purification of steam generator blowdown irrespective of the condition with Levoxin (hydrazine), ethanolamine or morpholine
  • removal of activated cleavage or corrosion products, including mechanical filtration of suspended impurities

Information provided by Lanxess.

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Bead Size, Mean, SBA
  • Bead Size, Mean, SAC
  • Storage Temperature
  • Shelf Life
  • Aluminum, Al, SAC; dry resin
  • Aluminum, Al, <40 mg/kg dry resin
  • Calcium, Ca, SAC; dry resin
  • Calcium, Ca, SBA; dry resin
  • Cobalt, Co, SAC; dry resin
  • Cobalt, Co, SBA; dry resin
  • Copper, Cu, SAC; dry resin
  • Copper, Cu, SBA; dry resin
  • Iron, Fe, SAC; dry resin
  • Iron, Fe, SBA; dry resin
  • Lead, Pb, Heavy metals (as Pb), SAC; dry resin
  • Lead, Pb, SAC; dry resin
  • Lead, Pb, SBA; dry resin
  • Lead, Pb, Heavy metals (as Pb), SBA; dry resin
  • Magnesium, Mg, SAC; dry resin
  • Magnesium, Mg, SBA; dry resin
  • Mercury, Hg, <1 mg/kg dry resin
  • SiO2, SAC; dry resin
  • SiO2, SBA; dry resin
  • Sodium, Na, SAC; dry resin
  • Sodium, Na, SBA; dry resin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.