MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ChevronTexaco RPM® SAE 10W-30 Heavy Duty Motor Oil
Categories: Fluid; Lubricant

Material Notes: Features:

Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocharged, and supercharged diesel engines in all types of service.

Chevron RPM Heavy Duty Motor Oils are priced for value with capabilities and performance that rival many of our competitor’s top tier products.

These multipurpose engine oils are manufactured using selected high viscosity index base oils and additives that provide maximum protection against sludge, varnish, ash deposits, wear, oxidation, foam, corrosion, and rust.

Chevron RPM Heavy Duty Motor oils SAE 15W-40 and 10W-30 are manufactured exclusively with Group II base oils.

Chevron RPM Heavy Duty Motor Oils provide excellent control of sludge formation(typical of cold engine operation).

They reduce deposit buildup resulting from high temperature engine operation, especially in the piston and ring area, combat varnish formation, and keep vital engine parts clean.

They flow readily at low temperatures for easier cold starting and less wear.

They also protect against corrosion and resist oxidation at high temperatures.

Chevron RPM Heavy Duty Motor Oils utilize the latest technology to provide excellent performance in both new and older model engines, using normal, high or low sulfur diesel fuels.

Applications:

Chevron RPM Heavy Duty Motor Oils are recommended for four-stroke gasoline engines, and all two- and four-stroke naturally aspirated, turbocharged, and supercharged diesel engines in all types of service. They are ideal for mixed commercial fleets, farm machinery, construction equipment, marine and other off-highway applications.

Chevron RPM Heavy Duty Motor Oils SAE 15W-40 and 30 can be used in powershift transmissions requiring Caterpillar TO 2 or Allison C4 fluids.

Chevron RPM Heavy Duty Motor Oil SAE 15W-40 meets the ECF-1 specification for Caterpillar’s ACERT™ engine technology.

API service categories

  • CI-4, CH-4, CG-4, CF-4 (SAE 15W-40, SAE 10W-30)
  • CF-2, CD-II (SAE 30, SAE 40, SAE 50)
  • CF, CD, SH, SG
  • SL, SJ (SAE 15W-40, SAE 10W, SAE 30, SAE 40, SAE 50)
  • CE (SAE 15W-40)

ACEA European Oil Sequences

  • E3-96 Issue 3, E5-99, B3-98 (SAE 15W-40)

Major diesel engine manufacturers’ requirements

  • Caterpillar ECF-1 (SAE 15W-40)
  • Cummins CES 20078, 20077, 20076, 20072 (SAE 15W-40)
  • Detroit Diesel Corporation Series 149 Engine (SAE 40, SAE 50)
  • DDC/MTU Series 2000 Category 1 and 2 (SAE 15W-40)
  • Engine Manufacturers Association (EMA) LRG-1 (SAE 15W-40, SAE 1-W-30)
  • Global DHD-1 (SAE 15W-40)
  • Man 3275 (SAE 15W-40)
  • MTU/DDC Series 4000 Category 1 (SAE 15W-40)
  • Mack EO-N Premium PLUS (SAE 15W-40), EO-M PLUS, EO-L PLUS, EO-L (SAE 15W-40, SAE 10W-30)
  • Mercedes Benz 228.3 (SAE 15W-40)
  • Volvo VDS-2 (SAE 10W)

Performance Requirements of

  • Allison C4 Fluids (SAE 15W-40, SAE 10W, SAE 30)
  • Vickers Pump Test (SAE 10W)

Manufacturers’ performance requirements

  • Chrysler MS 6395-G (SAE 15W-40)
  • Ford ESE-M2C153-E (SAE 15W-40)
  • General Motors GM 6094-M (SAE 15W-40, SAE 10W, SAE30, SAE 40, SAE 50)

Department of defense commercial item description (CID)

  • A-A-52306A2 (SAE 15W-40, SAE 30, SAE 40)
  • A-A-52039A3 (SAE 15W-40, SAE 10W-30)

Key Words: CPS Number: 225048; MSDS Number: 6931
Vendors:
Available Properties
  • API Gravity
  • Viscosity, Cold Crank
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Ash, Sulfated Ash wt%
  • Total Base Number, ASTM D2896
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  • Phosphorus, P
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.