MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Syensqo (Solvay Specialty Polymers) Amodel® AE-1133 PPA, 33% glass filled
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass filled, for Auto EE, heat stabilized

Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin.

- Black: AE-1133 BK 324
- Natural: AE-1133 NT

Applications: Automotive Electronics; Connectors; Electrical Parts; Electrical/Electronic Applications

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Injection notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ISO 1183, Method A
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength at Break, ISO 527-2
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Poissons Ratio, ASTM E132
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180, Type 1, Notch A
  • Izod Impact, Unnotched (ISO), ISO 180, Type 1
  • Charpy Impact Unnotched, ISO 179, Type 1, Edgewise
  • Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, UL 746
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Melting Point, ISO 11357-3
  • Melting Point
  • Maximum Service Temperature, Air, ASTM D794, Continuous
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Moisture Content, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.