Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in the grade nomenclature: Kraton D1153 AS - supplied as porous pellets dusted with amorphous silica Kraton D1153 AT - supplied as porous pellets dusted with talc Region: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1153 A is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings. Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing Information provided by Kraton® |