MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Melos Mecoline IS TP 1033 F Halogen-free, thermoplastic, highly flame retardant insulation and sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, highly flame retardant insulation and sheathing compound for low and medium voltage cables

Compound class: Insulation/Sheathing

Compound category: TP

Flame retardant: ATH

Standards: VDE 0207 part 24 HM2, HM4; DIN VDE 0276 part 604 HM4; IEC 60092-300 SHF 1; DIN VDE 0250 part 215 HM5

Typical applications: Halogen-free, low smoke, thermoplastic, highly flame retardant, UV-resistant compound for the insulation and sheathing of low and medium voltage cables in General Installation applications.

Features: Flame retardant; Halogen-free; Low smoke; Weather/UV resistant

Information provided by Melos

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1A, pressed plaques, 155°C / 5 min
  • pH, IEC 60754-2, Corrosivity
  • Melt Flow, DIN EN ISO 1133
  • Hardness, Shore D, DIN ISO 7619-1, pressed plaques, 155°C / 5 min
  • Tensile Strength, IEC 60811-501, extruded tapes
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, extruded tapes, Water purified
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, IEC 60811-404, extruded tapes, Water purified
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Penetration, IEC 60811-508, [%] Hot pressure test, extruded tapes
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94, Horizontal
  • Flammability, UL94, Vertical
  • Processing Temperature, Tool
  • Processing Temperature, Maximum mass temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Adapter Temperature
  • Head Temperature
  • Drying Temperature
  • Dry Time
  • Loss on Ignition(%), ASTM D 2863 A, pressed plaques, 155°C / 5 min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.