MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Melos Mecoline S TP 1039 F Halogen-free, thermoplastic, highly flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, flame retardant sheathing compound for data communications, low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: MDH

Standards: DIN EN 50363-8 TM7; DIN VDE 0276-604 HM4; DIN VDE 0281 part 14 TM7; IEC 60092-360 SHF 1; VDE 0207 part 24 HM2, HM4; VDE 0250 part 215 HM5; UL 1277 Oil Res I; UL 1277 Oil Res II; IEC 60502-1 ST8

Typical applications: Halogen-free, low smoke, thermoplastic, highly oil and extra fuel resistant, flame retardant compound for the sheathing of data communication, low and medium voltage cables for moving applications. (e. g. Telecomm/ Shipboard/Green Energy)

Features: Flame retardant; Halogen-free; Low smoke; Flexible; Flexible at low temperatures: Oil resistant

Information provided by Melos

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1A, pressed plaques, 155°C / 5 min
  • Melt Flow, DIN EN ISO 1133
  • Hardness, Shore D, DIN ISO 7619-1, pressed plaques, 155°C / 5 min
  • Tensile Strength, IEC 60811-501, extruded tapes
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, extruded tapes, Diesel
  • Tensile Strength, IEC 60811-404, extruded tapes, Diesel
  • Tensile Strength, IEC 60811-404, extruded tapes, Diesel
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-401, extruded tapes, After ageing in air oven
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, DIN EN ISO 527
  • Elongation at Break, DIN EN ISO 527
  • Elongation at Break, IEC 60811-404, extruded tapes, Diesel
  • Elongation at Break, IEC 60811-404, extruded tapes, Diesel
  • Elongation at Break, IEC 60811-401, extruded tapes, After ageing in air oven
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, extruded tapes, Diesel
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Penetration, IEC 60811-508, [%] Hot pressure test, extruded tapes
  • Tear Strength, BS 6469:99.1, extruded tapes
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature, Tool
  • Processing Temperature, Maximum mass temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Adapter Temperature
  • Head Temperature
  • Drying Temperature
  • Dry Time
  • Shelf Life
  • Loss on Ignition(%), ASTM D 2863 A, pressed plaques, 155°C / 5 min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.