MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Toray G-83CM Prepreg System - Resin Properties
Categories: Polymer; Thermoset

Material Notes: G-83CM resin system provides a quick cure (290°F for 20 min) or a low temperature cure (185°F for 6 hours) with the capability to achieve class “A” surface finish. This system works well for both autoclave and fast cycle press mold processes. Quick cure cycles are used where high-cycle applications are required; lower temperature cure applications would be used where mold material is heat sensitive. G-83CM is a proven system in the automotive industry due to its fast cure and high quality Class A capability. This system works well in a variety of other applications such as industrial and aircraft grade

Information provided by Toray Composite Materials America, Inc.

Vendors:
Available Properties
  • Density, ASTM D595
  • Storage Temperature, 24 months, Freezer Life
  • Storage Temperature, 3 months, Fridge Life
  • Tensile Strength, ASTM D3039, 90° (F2t), T700S-12K at 190 g/m2 FAW and 35% RC
  • Tensile Strength, ASTM D3039, 0° (F1t), T700S-12K at 190 g/m2 FAW and 35% RC
  • Tensile Modulus, ASTM D3039, 0° (E1t), T700S-12K at 190 g/m2 FAW and 35% RC
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Fracture Toughness, ASTM D5045-99, KIC
  • Shear Strength, ASTM D2344, Short Beam, T700S-12K at 190 g/m2 FAW and 35% RC
  • Shear Strength, ASTM D3518, ±45° In Plane, T700S-12K at 190 g/m2 FAW and 35% RC
  • CTE, linear
  • Glass Transition Temp, Tg, Dry
  • Cure Time, Ramp Rate: 5°F/min, Optional vent at 130°F, Cool Down Rate: 5°F/min
  • Gel Time, ASTM D3532
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.