Satisfactory finishing results can be obtained using carbide tipped tools. Applications include cutting plastics, rubber, paper, carpet, and wood; saw teeth, trimmer knives, carpet knives, ledger blades, rotary slitters, grid nozzles, burner tips, guide rolls, sleeves, bushings, and for protecting bearing surfaces, screw flights, and veneer pressure bars. Data provided by the manufacturer, Deloro Stellite, Inc.Product of former Deloro Stellite Inc. |
AWS A5.13 RCoCr-B, UNS R30012, AMS 7238, MIL-C-24248 COMP II, SAE J775 (VF7) |