MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Hippe PA 66 Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mechanical, automobile and plant engineering.

Information provided by Hippe.

Vendors:
Available Properties
  • Specific Gravity, DIN 53 479
  • Moisture Absorption at Equilibrium, DIN 53 715, Absorption of humidity in standard operating environment
  • Water Absorption at Saturation, DIN 53 495
  • Ball Indentation Hardness, DIN 53 456
  • Tensile Strength, DIN 53 455, cond.
  • Tensile Strength, DIN 53 455, dry
  • Elongation at Break, DIN 53 455, dry
  • Elongation at Break, DIN 53 455, cond.
  • Tensile Modulus, DIN 53 457, cond.
  • Tensile Modulus, DIN 53 457, dry
  • Flexural Modulus, DIN 53 457, from bending test
  • Charpy Impact, Notched, DIN 53 453
  • Coefficient of Friction, Dynamic, Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
  • Abrasion, µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
  • Volume Resistivity, DIN 53 482, VDE 0303, Part 3
  • Surface Resistance, DIN 53 482
  • Dielectric Constant, DIN 53 483, IEC-250
  • Dielectric Strength, DIN 53 481, IEC-243, VDE 0303 Part 1, Breakdown
  • Dielectric Loss Index, DIN 53 483, IEC-250
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, DIN 53 736
  • Maximum Service Temperature, Air, Continuous use
  • Maximum Service Temperature, Air, Short Periods
  • Deflection Temperature at 0.46 MPa (66 psi), ISO-R 75 Method B
  • Deflection Temperature at 1.8 MPa (264 psi), ISO-R 75 Method A
  • Glass Transition Temp, Tg, DIN 53 736, cond., dynamic
  • Glass Transition Temp, Tg, DIN 53 736, dry, dynamic
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Erhard Hippe KG

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.