MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Arla MULTICLEAR® BOX 2 WALL PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MULTICLEAR® BOX 2 WALL is an aesthetically pleasing twin wall extruded multiwall polycarbonate sheet which offers higher light transmission products with lower weight for handling and transportation. MULTICLEAR® BOX 2 WALL is transparent and translucent with one side UV protected sheet (also available with two side UV protection, except 4-6 mm). Standard colors are clear, opal and bronze. Available in thicknesses of 4, 6, 8 and 10 mm. Knife cutting operation is used both online and offline to avoid saw dust. MULTICLEAR® BOX 2 WALL has a 10 year limited warranty against discoloration, loss of impact strength and light transmission due to weathering.

Benefits: High light transmission; Excellent bending radius; One side UV protection as standard; Light weight - simple handling and installation

Application: Building industry – roofing, cladding, sidewalls, conservatories, domes, skylights, sheds, car ports, smoke vents, swimming pool covers, suspended ceilings, glasshouses, shopping center roofing, railway/metro station, stadia roofing and partitions. Lighting/packaging lamp optics and neon signs boxes, pallet shields, protective covers for fragile items. Advertising illuminated signs and advertising panels. Agriculture greenhouses, lorry/tractor ports and farm/barn buildings.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 50% RH
  • Hardness, Rockwell M, ISO 2039-2
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact Unnotched, ISO 179/2D
  • Charpy Impact Unnotched, ISO 179/2D
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, DIN 52612
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306, B 50
  • Vicat Softening Point, ISO 306, B 120
  • Refractive Index, ISO 489
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.