MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to reduce weight. The molybdenum and nitrogen additions have been optimized in order to obtain the best corrosion resistance properties even for heavy plates. Its high nitrogen content improves the structure stability particularly in HAZ. The CLI - SAF 2507® (URANUS® 47N+) grade is an overalloyed variant of the former UR 47N grade of CLI. CLI - SAF 2507® has improved corrosion resistance properties when compared to duplex 2205 type materials, or even to URANUS® 47N. It is designed for service in severe corrosive conditions. The alloy is particularly resistant to stress corrosion cracking and crevice corrosion. CLI - SAF 2507® is a cost efficient grade designed for Oil & Gas industry, Seawater applications, Desalination plants, Geothermal wells or Refineries and Petrochemical plants.

Information provided by manufacturer.

Key Words: EN 10088 - EN 10028.7 X2 Cr Ni Mo N 25.6.3 - 1.4410, AFNOR Z3 CND 25.07 AZ, ASTM A 240 - UNS S32750, SAF 2507
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C, Typical
  • Hardness, Vickers, Typical, V5
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Shear Modulus
  • Charpy Impact
  • Charpy Impact
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.