MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Versalis Riblene® FH 39 F Film Grade Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Riblene FH 39 F is a LDPE suitable for blown film extrusion. Riblene FH 39 D is characterized by a good balance between process ability and mechanical properties. Films manufactured by Riblene FH 39 D are easily heat shrinkable and have good optical and mechanical properties.

Application: Riblene FH 39 F is recommended for general packaging film and for diapers.

Property values reported for film extruded with BUR 1:3, thickness 70 µm. Actual properties are typical and may vary depending upon operating conditions and additive package.

Information provided by Versalis.

Vendors:
Available Properties
  • Density, ISO 1183
  • Thickness, Recommended
  • Thickness, As-tested; BUR 1:3
  • Melt Flow, ISO 1133
  • Film Tensile Strength at Yield, MD, ISO 527-3
  • Film Tensile Strength at Yield, TD, ISO 527-3
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Coefficient of Friction, Dynamic, ISO 8295
  • Elmendorf Tear Strength, MD, ISO 6383-2
  • Elmendorf Tear Strength, TD, ISO 6383-2
  • Dart Drop Test, ISO 7765-1/A, F50
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • 1% Secant Modulus, MD, ISO 527-3
  • 1% Secant Modulus, TD, ISO 527-3
  • Melting Point, Manufacturer method
  • Vicat Softening Point, ISO 306/A
  • Brittleness Temperature, ASTM D 746
  • Haze, ISO 14782
  • Gloss, ASTM D 2457, 45°
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polimeri Europa (Former Polimeri Europa (EniChem)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.