MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials Type 219 Fused Quartz Tubing  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Transmits the 253.7 nm mercury emission very efficiently, making it an ideal material for disinfecting applications and various other UV treatments. Softening point 1660°C. Annealing point 1204°C. Strain point 1106°C.

Data provided by GE Quartz.

GE Quartz became a part of Momentive Performance Materials in 2006.

Key Words: Quartz Tubes
Vendors:
Available Properties
  • Density
  • Viscosity
  • Knoop Microhardness, kg/mm²
  • Hardness, Mohs, (Type 214)
  • Modulus of Elasticity, Young's Modulus
  • Compressive Strength, design compressive strength
  • Electrical Resistivity
  • Dielectric Constant
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Softening Point
  • Annealing Point
  • Strain Point
  • Refractive Index
  • Transmission, Visible, Entire visible spectrum; 1 mm thickness (includes surface reflection losses)
  • IR Transmittance, Very wavelength dependent - drop begins above 2500 nm and cutoff almost complete at 4200 nm; (includes surface reflection losses)
  • UV Transmittance, Highly wavelength dependent - cutoff below 220 nm; (includes surface reflection losses)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GE Quartz - Momentive Performance Materials

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.