MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Wacker Wacker® Silane M2-DIETHOXY
Categories: Fluid

Material Notes: Empirical formula: C6H16O2Si

CAS No.: 78-62-6

Product description: Clear, colorless liquid. Dimethyldiethoxysilane hydrolyzes in contact with water to highly reactive silanols, which further condense to oligomeric and polymeric siloxanes. In general, precise pH control is important for the reproducibility of the hydrolysis, and the quality and stability of the hydrolysis product.

Application: WACKER® SILANE M2-DIETHOXY can be used:

  • for the synthesis of chemical intermediates
  • for hydrophobization of surfaces (glass, pigments)
  • as an additive for the production of silicone resins

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density
  • Viscosity, dynamic
  • Molecular Weight
  • Boiling Point
  • Flash Point, DIN 51755
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.