MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Huber HN 36 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: HN-36 is a halogen–free, medium-coarse particle size ATH product that provides low cost flame retardant and smoke suppression in a variety of applications. The particle size distribution is specifically designed for low viscosity, high filler loading levels, and excellent processing characteristics, up to 200°C.

Applications: HN-36 is recommended for rubber goods, compression molded thermosets, coatings, adhesives, latex, vinyl and urethane compounds and carpet backings.

Physical Form: White powder

Morphology: Hexagonal Platelets

Generic Type: Aluminum Hydroxide

CAS No.: 21645-51-2

Information provided by J.M. Huber Corporation

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density, packed
  • Brightness
  • Oil Absorption, 21 ml/100gm
  • Particle Size, Screen Analysis: 36.2 percent
  • Particle Size, Median Particle Diameter
  • Particle Size, Screen Analysis: 77.1 percent
  • Particle Size, Screen Analysis: 100 percent
  • Specific Surface Area, BET
  • Hardness, Mohs
  • Electrical Resistivity
  • Fe2O3
  • Free Water, TGA
  • Loss on Ignition(%)
  • Na2O, soluble
  • Na2O, total
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.