MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
LKAB Minerals MagnaDense 2 Fine Aggregate
Categories: Ceramic; Oxide

Material Notes: MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high density concrete. This heavy concrete is some 60% heavier than normal concrete and is easily produced and placed using standard equipment.

Minelco has its own in-house resources guaranteeing a long term reliable supply of consistent quality products. MagnaDense grades can be tailor made to specific customer requirements or purchased as standard grades.

Having a high particle density MagnaDense offers several advantages:

  • Reduced volumes = less excavation, transportation, reinforcement & time
  • Increased weight for a given volume
  • Reduced heat of hydration
  • High submerged/saturated density
  • High radiation shielding characteristics
  • Space saving
  • Noise and vibration dampening
  • Thermal energy storage

Applications: MagnaDense has a long history of use as construction material for both in-situ and precast applications.Loose ballast:
  • Offshore ballasting of rigs and caissons
  • Scour protection for underwater structures of pipelines
  • Ground stabilization - to reduce piling

Heavy concrete:
  • Under water concrete (tunnels, pipeline mattresses)
  • Counterweights (bridges, locks, sluices, elevators, excavators)
  • Coastal protection (breakwaters, precast antifer cubes)
  • Pipecoating (negative buoyancy coatings)
  • Radiation shielding (medical & nuclear)

MagnaDense is available in grades from 30 mm down to powder fineness, supplied from strategic stockpiles throughout Europe and the U.S.

The use of MagnaDense enhances the density of concrete. Full replacement of the local aggregate, both fine and coarse, makes it possible to reach a density of 4.0 t/m3, or interim densities by partial replacements.

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Hardness, Mohs
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Minelco Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.