MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Materion Silicon Aluminum (SiAl)™ Sputtering Target for Large Area Coating Applications
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Silicon Aluminum (SiAl) rotatable targets are reactively sputtered to obtain SiN and SiO2 layers. Due to their low index of refraction (~1.48), SiO2 layers are used in reflective and anti-reflective coating systems.

Benefits

  • Recycle program for backing tubes available in U.S.
  • Target material of extremely high homogeneity
  • Variety of target lengths and thicknesses available
  • Compositions beyond SiAl6-16wt% are available
  • Recycle program for backing tubes available
  • Metallic purities of >99.9% on request
  • Targets with customized composition, purity and microstructure available
  • Company dedicated to Quality Assurance and ISO 9001:2015 certified procedures.
Applications
Low-e Architectural Glass: SiN/SiO2 layers are embedded to protect the IR-reflecting silver layer from corrosion and to optimize the visual characteristics of the glass. SiN is often used as a scratch-resistant top coating due to its density and hardness.
Photovoltaic Applications: SiN/SiO2 function as a scratch-resistant layer with anti-reflective characteristics.

Information provided by Materion.

Vendors:
Available Properties
  • Density
  • Grain Size
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Calcium, Ca, <200 ppm
  • Chromium, Cr, <150 ppm
  • Copper, Cu, <150 ppm
  • Iron, Fe, <500 ppm
  • Nickel, Ni, <150 ppm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Materion Corporation (former Williams Advanced Alloys)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.