MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Henkel Loctite® 4502 Adhesive
Categories: Polymer; Adhesive

Material Notes: Product Description: LOCTITE® Product 4502 is a low viscosity, fast curing, single component cyanoacrylate adhesive. It is specifically formulated for difficult to bond substrates.

Typical Applications: Rapid bonding of a wide range of metal, plastic or elastomeric materials, particularly suited for bonding porous or absorbent materials such as wood, paper, leather or fabric

Information provided by Loctite®

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity, MK-22 Cone
  • Shear Strength, ASTM D1002, Nitrile rubber
  • Shear Strength, ASTM D1002, Neoprene rubber
  • Shear Strength, ASTM D1002, Zinc dichromate
  • Shear Strength, ASTM D4501, Phenolic
  • Shear Strength, ASTM D1002, Grit Blasted Aluminum
  • Shear Strength, ASTM D4501, PVC
  • Shear Strength, ASTM D1002, Grit Blasted Steel
  • Shear Strength, ASTM D4501, Polycarbonate
  • Shear Strength, ASTM D4501, ABS
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Glass Transition Temp, Tg, ASTM E228
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.