FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr017-D is subject to the specific limitation that it may contact food only at temperatures of 212°F and below. NOVA Chemicals' polyethylene resins are chemically and biologically inert. Features: Outstanding melt strength, Superior toughness with excellent tear strength, Excellent seal properties, Low gel Additives: Process stabilizer, Polymer process aid, Antiblock, Slip Applications: Industrial liners, Retail trash bags, High toughness film Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and a 35-mil die gap at a blowup ratio of 2.5:1, but are dependant upon operating conditions. |