MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phosphor bronze 8% Sn, UNS C52100, HR06 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Extra Hard and Stress Relieved

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld; Good Suitability – Gas Shielded Arc Welding, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Shearing; Stamping

Typical uses: Bridge Bearing Plates; Thermostat Bellows; Coinage; Power Conductor for Electro-Surgical Pencil; Cold Headed Parts; Electrical Connectors; Electrical Flexing Contact Blades; Electronic Connectors; Fuse Clips; Switch Parts; Wire Brushes; Cotter Pins; Fasteners, Heavy Duty; Lock Washers; Beater Bar; Bellows; Bourdon Tubing; Chemical hardware; Clips, Heavy Duty; Clutch Disks; Cold Headed Parts; Diaphragms; Doctor Blades, Paper Industry; Gears; Perforated Sheets; Pinions; Pneumatic Hammers; Sleeve Bushings; Springs, Heavy Duty; Springs, Helical Extension; Springs, Helical Torsion; Textile machinery; Thrust Bearings; Truss Wire; Welding Wire; Well Drill Equipment; Marine Parts

Applicable Specifications: Bar – ASTM B139/B139M, ASTM B103/B103M; Electrode – Welding AWS A5.6, Welding MILITARY MIL-E-23765/3; Plate – ASTM B103/B103M; Rod – Welding AWS A5.15, ASTM B139/B139M; Shapes – ASTM B139/B139M; Sheet – ASTM B103/B103M, SAE J463, SAE J461; Strip – ASTM B888/B88M; SAE J463, ASTM B103/B103M, SAE J461; Wire – ASTM B159/B159M

Vendors:
Available Properties
  • Density
  • Tensile Strength
  • Tensile Strength, Yield, 0.2% Offset
  • Elongation at Break
  • Tensile Modulus
  • Modulus of Rigidity
  • Poissons Ratio, Calculated
  • Machinability
  • Electrical Resistivity, 13% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Copper, Cu, As Balance
  • Iron, Fe
  • Lead, Pb
  • Phosphorus, P
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.