MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Categories: Ceramic; Carbide; Ceramic Matrix Composite

Material Notes: Engineered ceramic composite structures for a broad range of industries and applications.

Reinforcing Fiber Flexibility: S300 - Sylramic SiC
Preceramic Polymer Matrix Precursors: S300 - Crystalline (SiC + Si3N4) or SiC
Physical Attributes: Dense Matrix (<5%), High Temperature Capability, Good Matrix Dominated Properties and Wear Resistance

Typical Applications: Commercial Aviation Exhaust, Military Aircraft Propulsion Exhaust, Industrial

Produced using the Polymer Impregnation & Pyrolysis (PIP) process. This versatile and robust process is well suited for the fabrication of complex components. The PIP process utilizes a combination of polymeric and ceramic processes, combining a variety of ceramic fibers, fillers and pre-ceramic polymer resins to produce engineered ceramic composite structures for a broad range of industries and applications.

Process temperatures referenced in property table: T1< T2 < T3 < T4.

Information from COI Ceramics, Inc.

Vendors:
Available Properties
  • Tensile Stress at Strain, Process Temperature T4
  • Tensile Stress at Strain, Process Temperature T1
  • Tensile Stress at Strain, Process Temperature T2
  • Tensile Stress at Strain, Process Temperature T3
  • Tensile Stress at Strain, Process Temperature T4
  • Tensile Stress at Strain, Process Temperature T1
  • Tensile Stress at Strain, Process Temperature T2
  • Tensile Stress at Strain, Process Temperature T3
  • Tensile Stress at Strain, Process Temperature T4
  • Tensile Stress at Strain, Process Temperature T1
  • Tensile Stress at Strain, Process Temperature T2
  • Tensile Stress at Strain, Process Temperature T3
  • Tensile Stress at Strain, Process Temperature T4
  • Tensile Stress at Strain, Process Temperature T1
  • Tensile Stress at Strain, Process Temperature T2
  • Tensile Stress at Strain, Process Temperature T3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.