MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Polymer Tailoring PTFA 07 Polypropylene compound
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PTFA 07 is a new generation of halogen-free, highly stabilized polypropylene compound for injection moulded applications. The main features include ease of moulding, excellent UV and thermal stabilities, low specific gravity and a flammability rating to UL 94 V0 at 3.2mm.Examples of suitable applications range from electrical sockets and boxes to internal light fittings, plus other areas where a combination of high UV stability and thermal oxidative stability is required. A service temperaturein air of 100ºC over a period of months to years (i.e. medium term) is within expectation. Articles made from this compound will meet the environmental criteria of both the WEEE and ROHS Directives, as PTFA07 is 100% environmentally-friendly.
  • Easy to mould
  • Very flexible and strong
  • Very high impact strength
  • PP copolymer based
  • High thermal and UV stabilities
  • Lower processing temperature(~180ºC) allows for energy savings in production
  • Lower density (specific gravity)means more units per tonne
Currently Available Colours: White

Information provided by Polymer Tailoring Ltd.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Izod Impact, Notched (ISO), ISO 180
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ASTM D 2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.