MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
AISI Type S45500 Stainless Steel, hardened at 540°C (1000°F) for 4 hours, air cooled
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Martensitic, age-hardenable, easily formable (annealed), no corrosion in fresh water, resists staining in normal air atmosphere, good resistance to pitting in 5% salt spray and 5% ferric chloride. For use in service temperatures up to 425°C.

Key Words: UNS S45500, AMS 5578, AMS 5617, AMS 5672, AMS 5860, ASTM A313 (XM-16), ASTM A564 (XM-16), ASTM A705 (XM-16), martensitic, T S45506
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Converted from Rockwell C hardness. Strip
  • Hardness, Brinell, Converted from Rockwell C hardness. Strip
  • Hardness, Brinell, Converted from Rockwell C hardness. Bar
  • Hardness, Brinell, Converted from Rockwell C hardness. Bar
  • Hardness, Knoop, Converted from Rockwell C hardness. Strip
  • Hardness, Knoop, Converted from Rockwell C hardness. Strip
  • Hardness, Knoop, Converted from Rockwell C hardness. Bar
  • Hardness, Knoop, Converted from Rockwell C hardness. Bar
  • Hardness, Rockwell C, Strip
  • Hardness, Rockwell C, Strip
  • Hardness, Rockwell C, Bar
  • Hardness, Rockwell C, Bar
  • Hardness, Vickers, Converted from Rockwell C hardness. Strip
  • Hardness, Vickers, Converted from Rockwell C hardness. Strip
  • Hardness, Vickers, Converted from Rockwell C hardness. Bar
  • Hardness, Vickers, Converted from Rockwell C hardness. Bar
  • Tensile Strength, Ultimate, Strip
  • Tensile Strength, Ultimate, Strip
  • Tensile Strength, Ultimate, Bar
  • Tensile Strength, Ultimate, Bar
  • Tensile Strength, Yield, Strip
  • Tensile Strength, Yield, Strip
  • Tensile Strength, Yield, Bar
  • Tensile Strength, Yield, Bar
  • Elongation at Break, in 50 mm. Strip
  • Elongation at Break, in 50 mm. Strip
  • Elongation at Break, in 25 mm. Strip
  • Elongation at Break, in 25 mm. Strip
  • Elongation at Break, in 50 mm. Bar
  • Elongation at Break, in 50 mm. Bar
  • Modulus of Elasticity, Typical for stainless steel
  • Notched Tensile Strength, Bar
  • Notched Tensile Strength, Bar
  • Charpy Impact, Bar
  • Charpy Impact, Bar
  • Electrical Resistivity, annealed, 0.000075 Ohm-cm when annealed and aged at 510°C for 4 hours and air cooled.
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity, Typical value for stainless steel.
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.