MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger are available in three grades: TECATOR™ TI 5013, high strength structural grade featuring good electrical properties and strength, making it ideal for demanding applications at a broad range of temperatures. TECATOR™ TI 5031 offers high PV capabilities in bearing applications, primarily at high loads and low speeds. TECATOR™ GF30 (XP1424T) is a 30% glass filled grade, compression molded with superior stiffness and dimensional stability. It is available in a wide variety of custom tube, ring, rod and plate sizes.

  • Excellent weather and gamma radiation resistance
  • Outstanding bearing wear properties (at elevated temperatures, TECATOR™ TI 5031 offers superior wear rates)
  • High strength and stiffness
  • Excellent electrical values
  • Good chemical resistance (TECATOR™ is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)
  • Maintains a high proportion of mechanical properties over a broad temperature spectrum - cryogenic to 500°F
  • TECATOR™ TI 5013 and TI 5031 are available in a wide variety of metric sizes in rod and plate

TECATOR™ (PAI) typical applications: Pump parts, valve seats, piston rings, seal rings, engine transmission parts and bearing cages. For the semiconductor industry it is used for "burn in" test sockets, nests, chassis and other applications such as welding nozzle tips.

Information Provided by Ensinger Industries, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695, 1% offset
  • Izod Impact, Notched, ASTM D256
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor
  • Dissipation Factor
  • Dissipation Factor
  • CTE, linear, ASTM D696
  • Maximum Service Temperature, Air, continuous
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.