MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Morgan Advanced Ceramics Firemaster Board 550 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Alkaline Earth Silicate. Made exclusively from low bio-persistent alkaline earth silicate (AES) fibres, refractory fillers and selected binders, this board is recommended for fire protection of structural elements where high strength and good machinable properties are required. FireMaster® 550 board is available in large panel sizes and has good screw holding strength making it ideal for the construction of walls, ceilings and partition systems. FireMaster® 550 board has advantages of lower weight and lower thermal conductivity than calcium silicate boards together with the benefit of water repellence. In addition, ireMaster® 550 board has low dust emission during cutting operations.

Applications:

  • Structural steel fire protection (FireMaster® 550 board)
  • Fire damper systems insulation (FireMaster® 550 board)
  • Core material for fire rated decorative veneered panel systems
  • Ducting system

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Absorption Coefficient, test to BS EN 20354: 1993 Method
  • Modulus of Rupture
  • Compressive Strength, 10% reduction in thickness
  • Thermal Conductivity, ASTM C-201-68
  • Thermal Conductivity, ASTM C-201-68
  • Thermal Conductivity, ASTM C-201-68
  • Thermal Conductivity, ASTM C-201-68
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.