MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Go Yen Chemical GGK-1402 Anti-Scratch & Wear-Resistant & Coupling Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GGK-1402 is an anti-scratch & wear resistance & coupling agent for ink coating resins developed by GO YEN CHEMICAL INDUSTRIAL CO. LTD. (GYC GROUP). It can be widely used in surface printing, spraying and industrial applications such as ink, paint, resin, ceramics and plastics. GGK-1402 has unique wear and scratch resistance, effective adhesion, good processability and dispersibility, it is especially suitable for processing of coatings and resins. For ink coating systems of high water resistance requirements, GGK-1402 can significantly improve the water resistance, improve the weatherability and delay the pulverization. In addition, GGK-1402 can reduce the phenomenon of ink coating precipitation, combine with solvents and ingredient, improve the mechanical strength and surface gloss of the coating. GGK-1402 is also the most suitable anti-scratch, wear-resistant and coupling agent for ink coatings, and was used by many ink coatings and resin factories in the world.

Advantages:

  • Anti-scratch & wear resistance agent for surface treatment
  • Improve antiseptic and wear resistance of inks and coatings.
  • Good anti-scratch & wear resistance for various inks and synthetic resin products.
  • Very fine powder, excellent dispersion.
  • Anti-cracking for coating, improve the mechanical properties.
  • Good suspension in aqueous and oily systems.
  • GGK-1402 can reflect light and heat and reduce the
  • damage of coating by ultraviolet light and other light and heat.
  • Improve the weather resistance, water permeability, acidbase resistance and high temperature resistance for the coating
  • Prevent precipitating for ink and paint.
  • Low surface tension, added to inks and coatings can remove defects caused by grease and release agent contamination
  • Enhance the adhesion of the coating and improve the appearance of the coating
Applications:
  • TPU, PU
  • Various water and oil system inks, coatings, resins.
  • Spraying, inkjet, and coating of packaging materials.
  • Ink for flexographic printing or gravure printing.
  • Inkjet printing ink, offset ink, Screen printing ink.
  • Used for spraying, printing, 3D printing PC, PE, PP, rigid PVC, and various plastic materials.
  • Used to print thermosetting plastics, metals, painted substrates, and enhanced the chemical, mechanical resistance and adhesion.
  • For long-term outdoor use: advanced self-adhesive film, advertisements, stickers, etc. Suitable for high speed machine printing, including multi-roller presses.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Oil Absorption
  • pH
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.