MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Sumitomo Bakelite Varcum 29008 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29008 is a non-heat reactive, alkyl-substituted, solid phenolic resin supplied in flake form.

APPLICATIONS:

  • Tackifier for chlorobutyl rubber in white sidewall and tire inner liner compounds.
  • Tackifier for SBR, butyl and other synthetic rubbers.
  • Recommended for the production of high grade oleo resinous varnishes.
  • Can be used directly, or for blending with alkyd resins.
  • Varnishes formulated utilizing this resin may be used as vehicles in pigmented enamels.
  • Not recommended for white or very light colored enamels.
  • Contains no modifying agents and is suitable for use with any of the typical drying oils used in varnish formulations.
  • Good gas proofing characteristics.
  • Varnishes exhibit excellent drying characteristics and dried films have exceptional resistance to alkalies and water.
  • For optimum control, varnish cooks of the dispersion type are recommended.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors:
Available Properties
  • Softening Point, DCT 4000A, B&R
  • Gardner Color Number, DCT 4075A, G-H
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Durez Corporation; Sumitomo Bakelite High Peformance Plastics, SBNA, SBHPP

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.