MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or 3. Adhesive wear is similar to Stellite alloy 6, but resistance improves as the load increases. Galling resistance is excellent. The alloy is brittle and withstands less impact than either Stellite alloy 6 or 12. This material is suitable for high temperature abrasion in corrosive environment.

Stellite Alloy 4 has higher corrosion resistance than Stellite alloy 6 in oxidizing environments such as nitric and sulphuric acids. This improvement is due to the higher chromium content in the cobalt rich matrix making this material suitable for pump components. The alloy has excellent resistance to manganese dioxide, carbon particles and ammonium and zinc chlorides, used in the manufacturing of dry batteries. Corrosion resistance will vary depending on acid concentration, temperature, stress and contamination thus production exposure tests are recommended. This material does not respond to thermal treatments but may be stress relieved before and during machining by holding at 1650°F for 4 hours and slow cool.

Applications involve corrosion and wear such as pump sleeves and impellors. For high temperature wear the material has been used for dies in hot pressing or extrusion of copper and aluminum. The modified alloy Stellite 4B resist abrasion and corrosion from manganese dioxide, carbon particles and ammonium and zinc chlorides used in the dry battery industry.

Information provided by Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Ultimate Compressive Strength
  • Izod Impact Unnotched
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Nickel, Ni
  • Silicon, Si
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Kennametal Stellite, former Deloro Stellite Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.