Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
AGC Fluon® P-62XP PFA Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Fluon® PFA (perfluoroalkoxy) is a melt-processible copolymer of tetrafluoroethylene and a perfluorinated vinyl ether. Fluon® PFA has chemical, electrical, and thermal properties almost identical to its close chemical cousin, polytetrafluoroethylene (PTFE), yet can be processed by conventional extrusion, injection molding, blow molding, and transfer molding techniques. This material can be used over a wide range of temperatures (-200°C to 260°C). It is available as a 1/8” pellet.

Benefits:

  • High Resistance to Heat
  • Excellent Chemical Resistance
  • Low Smoke and Flame Characteristics. Fluon® PFA is rated 94V-0 by Underwriters Laboratories Inc.
  • Outstanding Resistance to Weather and Aging
  • Excellent Dielectric Properties
  • Non-Stick Characteristics
Applications:
  • Tubing and Pipe
  • Film and Sheets
  • Valves, Fittings, and Housings
  • Wire and Cable

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Melt Flow, ASTM D3159
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638
  • Tensile Strength, ASTM D638
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus
  • Flexural Modulus
  • Flex Crack Resistance, ASTM D2176, Cycles per MIT Folding Endurance
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM C256
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • Specific Heat Capacity
  • Melting Point, ASTM D3459
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, JIS K7206, 50°C/h
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.