Product Description: ANOX™ PP18 stabilizer is a high molecular weight hindered phenolic antioxidant available in both powder and granular form Application: ANOX™ PP18 stabilizer effectively reduces oxidative degradation of most polymeric substance during processing and end-use applications. ANOX™ PP18 stabilizer is an excellent stabilizer fro polyolefins, impact modified styrenics, block co-polymers, elastomers, adhesives, PVC and polyurethanes. CAS No: 2082-79-3 EINECS No: 218-216-0 Information provided by Akrochem Corporation |