Cure: Heat cure
Product Benefits:
Filler Type: Silica
Typical Package Application: Die to die stack
Carrier Type: Polyolefin
LOCTITE ABLESTIK ATB 120U adhesive film is formulated for use in wafer lamination processes. It combines process ease with the proven reliability.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic