MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
AGC Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Modified ETFE, Unreinforced

Material Notes: Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive agent or surface treatment that is used at previous system. Excellent adhesiveness of the two-layer system is effected for only one step. Furthermore, the conventional properties such as anti stick, excellent moldability and chemical resistance, are same as conventional fluoro-resin.

Information provided by Asahi Glass Company, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D359
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Surface Resistivity per Square
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.