MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Arla SAPHIR® PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: SAPHIR® is hard coated polycarbonate sheet with glass like appearance suitable for flat applications. The high impact strength of polycarbonate is combined with improved weather and chemical resistance. The product offers protection against abrasion compared to standard plastic sheets. SAPHIR® is resistant to many of the most common chemicals, and the hard coat also provides an excellent protection against graffiti and vandalism. SAPHIR® weighs about half of standard glass, yet the product is virtually unbreakable. SAPHIR® has an outstanding clarity, the hard coat improves the light transmission of the polycarbonate sheet.

Benefits: Abrasion and Impact Resistant; Chemical Resistance; UV Stability; High optical quality and outstanding clarity; More than 10 times the impact strength of high impact PMMA

Application: Anti-vandal glazing, security glazing, safety screens and acoustic screens, Industrial equipment (machine coverings, machine protections), Indoor and outdoor signs, vending machine faces and many different kinds of technical parts.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 50% RH
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Abrasion, ASTM D1044, % Haze; Taber, CS 10F, 500 cycles
  • Abrasion, ASTM D1044, % Haze; Taber, CS 10F, 500 cycles
  • CTE, linear, ISO 11359-2
  • Thermal Conductivity, DIN 8302
  • Refractive Index, ISO 489
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.