MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Hifax™ RTA3263/2 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impact strength and paintability. It was designed primarily for rigid automotive exterior ornamentation applications. Uses: Automotive exterior parts

Information provided by Basell.

Vendors:
Available Properties
  • Density, ISO 1183 & ASTM D792
  • Linear Mold Shrinkage, ASTM D955, 0.125 in
  • Melt Flow, ASTM D1238, Condition L
  • Hardness, Shore D, ISO 868 & ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ISO 527-1, -2
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ISO 527-1, -2 & ASTM D638
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Gardner Impact, ASTM D3029, tested in accordance with ASTM D5420
  • Dart Drop, Total Energy, ASTM D3763, Instrumented Energy at Maximum Load, Ductile Failure
  • Tear Strength, ASTM D624
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1, -2, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75A-1, -2, Unannealed
  • Shrinkage, Basell Test Method, Tool, 100x150x3.2 mm
  • Shrinkage, Basell Method, Afterbake, 100x150x3.2 mm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.