MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Zell-Metall Engineering Plastics Zellamid 1100 OIL
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces friction in comparison to standard cast nylon.

This means that Zellamid® 1100 OIL is particularly well suited for sliding parts under high load and increased speed.

The specific advantages of Zellamid® 1100 OIL against Zellamid® 1100 are:

  • High degree of self lubrication.
  • Low static coefficient of friction.
  • Low dynamic coefficient of friction.
  • Reduced heat build-up.
  • Better wear and enormously increased part life due to less heat build-up in the area of friction.
  • Reduced moisture absorption (about 5% for Zellamid® 1100 OIL vs. 6-7% for Zellamid® 1100).
  • Increased dimensional stability.
Zellamid® 1100 OIL features a homogeneous distribution of the lubricating oil during polymerization. Therefore the improved sliding properties remain, even after machining and part wear. The p. v. value may be used as a guideline to determine the loading capacity of slide bearings at a certain velocity. The values mentioned in the attached data sheet apply for the material combination of Zellamid® and metal for continuous use when heat is well conducted and environmental temperature is normal. Higher are permissible when on is intermittent.

When using additional lubricants with Zellamid® 1100 OIL, the external lubricant influences the coefficient of friction to a very high degree. It can be reduced to 0.05. Consequently, the p. v. value may be increased. The advantages of the integrated lubrication of Zellamid® 1100 OIL are particularly noticeable when there is a combination of static and dynamic friction, especially when external lubrication is insufficient or impossible. Zellamid® 1100 OIL is supplied in yellow color for easy identification.

Vendors:
Available Properties
  • Density
  • Moisture Absorption at Equilibrium, 50% RH
  • Water Absorption at Saturation, 23°C
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, DIN 53456
  • Tensile Strength at Break, DIN 53455
  • Elongation at Break, DIN 53455
  • Tensile Modulus, DIN 53457
  • Tensile Modulus, DIN 53457
  • Charpy Impact Unnotched, DIN 53453
  • Charpy Impact, Notched, DIN 53453
  • Coefficient of Friction, to steel, added lubrication
  • Coefficient of Friction, ISO/DTR 7147, to steel, no lubrication
  • Abrasion, DIN 53516, mm³
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, DIN 52612
  • Melting Point
  • Maximum Service Temperature, Air, long time operation
  • Maximum Service Temperature, Air, medium time operation
  • Maximum Service Temperature, Air, a few hours operation
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.