AA-BOND FDA26 is Versatile adhesive guaranteed a high strength bond. AA-BOND FDA26 is two part adhesive used and cured at room temperature for bonding, repair applications by manufacturers of food preparation, processing and packaging equipment and devices. Appearance: Gray Cure Type: Heat cure or Room Temperature Benefits: - Excellent durability
- High shear and peel strength
- Heat and impact resistant
- Handy duo-pack cartridges for easy mixing
Mix Ratio by weight: 100:14/Resin:HardenerSubstrates: Most metals, ceramic, glass and plastics Information provided by Atom Adhesives |