Chlorinated polyethylene is a heat, weathering and oil resistant elastomer that has used in many wire/cable, hose, automotive and industrial parts for many years. Characteristics: Highest molecular weight, relatively narrow molecular weight distribution, highest Mooney viscosity and best mechanical property Application: High viscosity grade for highly filled hose, cable jackets, HPN cords, sponge and molded products. Information provided by Sundow Polymers Co., Ltd |