General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine. Applications: Pentfoam 193L is particularly well suited for hte manufacture of eps low density insulation boards from block molding. This grade is always widely used for the production of low density decoration products, and drainage boards. |