MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Data provided by the manufacturer.

HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.

Key Words: Ethylene Chlorotrifluoroethylene Copolymer
Vendors:
Available Properties
  • Density
  • Water Absorption, 168 hours
  • Moisture Absorption at Equilibrium, after 168 hours
  • Hardness, Rockwell R
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Yield Strength
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Notched
  • Tensile Impact Strength, ASTM D1822S
  • Coefficient of Friction, Dynamic, vs. steel; 50 cm/s (20 in/s); ASTM D1044
  • Coefficient of Friction, Static, vs. steel; ASTM D1044
  • Taber Abrasion, mg/1000 Cycles, CS-17 wheels; 500 g; wheels cleaned every 25 cycles
  • Electrical Resistivity
  • Surface Resistance, ASTM D257
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dielectric Strength
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor
  • Arc Resistance, ASTM D495, Test Terminated at 50 sec.
  • Comparative Tracking Index
  • Hot Wire Ignition, HWI
  • High Amp Arc Ignition, HAI, test terminated at 200 arcs 1/16 A.S.
  • High Voltage Arc-Tracking Rate, HVTR
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, Halar® 300
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Brittleness Temperature
  • Flammability, UL94
  • Oxygen Index
  • Refractive Index
  • Haze, typical for HALAR films; ASTM D1003
  • Gloss, 85-95% at 20° is typical of HALAR films; ASTM D2457
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.