MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resistance properties when compared to 13 Cr ferritic-martensitic grades (AISI 410-420/Euronorms 1.4000 X6 Cr 13). The alloy has good corrosion resistance to fresh water and performs well under erosion-corrosion phenomena. The alloy is specially designed for all applications requiring high mechanical properties combined with high toughness and may be used in medium corrosive conditions. Typical applications are shafts or compressor impellers, particularly for hydraulic applications.

Information provided by manufacturer.

Key Words: EURONORM 1.4313-X4 Cr Ni Mo 13-4, AFNOR Z4 CN13.4, DIN X5 Cr Ni 13-4 W.Nr. 1.4313, AISI 41500
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Typical
  • Tensile Strength, Ultimate, Minimum Guaranteed
  • Tensile Strength, Yield, Minimum Guaranteed
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Shear Modulus
  • Charpy Impact
  • Charpy Impact, Typical
  • Charpy Impact
  • Charpy Impact, Typical
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.