MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Teknor Apex SarlinkĀ® TPE EE-2740D NAT Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-2740D NAT is a high performance thermoplastic elastomer designed for automotive applications, including exterior trim. Sarlink EE-2740D NAT is a high hardness, low density extrusion grade that is light stabilized and sunlight resistant.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: High Hardness; Light Stabilized; Low Density; Low Flow; Low Specific Gravity; Slip; Sunlight Resistant; Without Fillers

Uses: Automotive Applications; Automotive Exterior

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-DC-242 CPN4707

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, ASTM D3835
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240, Injection Molded
  • Hardness, Shore D, ASTM D2240, Injection Molded
  • Tensile Strength at Break, ASTM D412, Across Flow
  • Tensile Strength at Break, ASTM D412, Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Stress at Strain, ASTM D412, Across Flow
  • Tensile Stress at Strain, ASTM D412, Flow
  • Elongation at Break, ASTM D412, Flow
  • Elongation at Break, ASTM D412, Across Flow
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Gardner Impact
  • Tear Strength, ASTM D624, Across Flow
  • Compression Set, ASTM D395
  • Compression Set, ASTM D395
  • Compression Set, ASTM D395
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 5
  • Die Temperature
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.