MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Solvay LTM® 123 Cyanate Ester Prepreg with AS4 Reinforcement
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: LTM123 is a low temperature curing, toughened cyanate ester component prepreg developed for structural applications requiring ultimate dimensional stability in a space environment. Its low moisture absorption and low electrical permittivity characteristics also make it suitable for radomes and radar absorbing structures. LTM123 is also suitable for high service temperature structural applications in the motorsport market. LTM123 can be processed using autoclave and oven vacuum bag methods to produce low voidage composites and can be molded off a range of low cost tooling with few constraints on structure dimensions. For space applications, LTM123 can develop a Tg of 140LC (248°F) after a minimum initial cure at 80°C (176°F) and a free-standing post-cure of 120°C (248°F). For motorsport applications, LTM123 can develop a Tg of 250°C (482°F) after a minimum initial cure at 80°C (176°F) and free-standing post-cure of 240°C (464°F).

Features & Benefits:

  • 3 days tack life at 21°C (70°F)
  • 6 months storage at -18°C (0°F)
  • 70°C (158°F) initial cure
  • Autoclave cure
  • Good dimensional stability and thermal durability up to 250°C (482°f) after post-cure
  • Maximum Tg of 330°C (626°F); can withstand thermal spikes to 330°C (626°F)
  • Inherently flame retardant, with low toxic gas and smoke generation
  • Good dielectric properties for radar transparency
Property data reported for: LTM123/AS4; Cure: 16 hrs at 80°C (176°F), 6.2 bar (90 psi); Post-cure: 2 hrs at 175°C (347°F). Compressive and tensile properties normalized to 60 vol%.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Moisture Absorption at Equilibrium, 0 to 60% RH, 60°C, (1.5mm 0°±60°C M55J reinforcement)
  • Storage Temperature, LTM® 123
  • Flexural Strength, CRAG 200, 0°, dry
  • Flexural Modulus, CRAG 200, 0°, dry
  • Compressive Strength, ASTM D3410, 0°, dry
  • Compressive Strength, ASTM D3410, 0°, wet; immersed 14 days at 70°C
  • Shear Strength, ASTM D2344, 0° Interlaminar. dry
  • Shear Strength, ASTM D3518, ±45° In-plane, dry
  • CTE, linear, 0°; M55J reinforcement
  • Cure Time, Post-cure As Tested
  • Cure Time, As Tested
  • Shelf Life, LTM® 123
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.