MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP3LV One Component Heat Curing Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Description: Master Bond EP3LV represents a breakthrough in epoxy adhesive technology featuring a hitherto unattainable balance of performance properties including both high shear and high cure speed. This one component adhesive system is formulated to cure at elevated temperatures, e.g., 5-10 minutes at 300- 325°F, longer times at lower temperatures for maximum bond strengths. Tensile strengths in excess of 2000 psi are readily obtained after such short cure times. No mixing is necessary prior to use. EP3LV produces truly exceptionally good performance bonds with durable high lap shear strength for service in the remarkably wide temperature range of -100°F to +300°F. It offers superior resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and thermal resistance typical of epoxy resin adhesives. It is 100% reactive and does not contain any diluents or solvents. EP3LV produces durable high strength, exceptionally tough bonds which are remarkable resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents even upon prolonged exposures. For best results all surfaces should cleaned and then either roughened or chemically etched. Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is a superior thermal insulator. The color is gray. EP3LV offers the convenience of a heat cure with no mixing prior to use and uniquely favorable bonding performance for even the most difficult applications in the aerospace, electronic electrical computer, metalworking, appliance, automotive and chemical industries.

Product Advantages:

  • Single component system; no mixing prior to use. Unlimited working life at room temperature.
  • Easy application; contact pressure only required during simple heat cure; adhesive spreads evenly and smoothly.
  • Versatile cure schedules: 5-10 min at 300-325°F, longer time periods at lower temperatures as desired. Minimum curing temperature, 235°F.
  • High tensile shear strength to similar and dissimilar substrates over the wide temperature range of -100°F to +300°F.
  • Good electrical insulating properties and chemical resistance.
  • Superior thermal shock; impact and stress cracking fatigue resistance.
  • Superior durability and dimensional stability.

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Solids Content
  • Viscosity
  • Storage Temperature
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.