Forms: Pellets
Filler/Reinforcement: Carbon Fiber, 30% Filler by Weight
Additive: PTFE Lubricant(15%) and Heat Stabilizer
Features: Lubricated, Good Wear Resistance, Heat Stabilized and Low Friction
Appearance: Black
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide