MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Eastman Cristal™ EN067 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ copolyester EN067 is a copolyester designed to be fully compatible with the PET recycling stream. It enables recyclable cosmetics packaging with a combination of good color and high clarity for molded parts with an RIC1 resin. This product is suitable for thinner-walled molded parts for the cosmetics and personal care market. Cristal™ EN067 meets the definition of resin identification code #1 (RIC1) as defined by California Assembly Bill (#906) and by ASTM D7611. Other end-product attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability.

Applications

  • Bottles-color cosmetics pkg
  • Bottles-skin care pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Ease of processing
  • Good chemical resistance
  • Good flow
  • Good toughness
  • High clarity
  • Neutral color in a RIC1 resin
  • Recyclable with the PET stream

Information provided by Eastman.

Vendors:
Available Properties
  • Density, ASTM D792
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Transmission, Visible, ASTM D1003, Regular
  • Transmission, Visible, ASTM D1003, Total
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.