Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhibits good toughness, superior biaxial stretchability, and flexibility even at low temperatures. It is insensitive to stress cracking and notch effects. Special stabilization provides good resistance to heat ageing and UV radiation. Lucolit is thus to a large extent resistant to weathering and ageing. Applications: • Roofing sealing and membranes • Construction profiles and water stops • Injection molded parts in the building sector Information provided by Lucobit AG |