MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel Superplast® 400 High Hardness Mold Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Mold Steel

Material Notes: SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty molds used for production of long series, for compression molds or when an improved wear resistance is expected. SUPERPLAST® 400 will be ideal where a high resistance of the mating plan surface is required and when the conventional 300 HB or even conventional high hard material cannot ensure adapted properties. SUPERPLAST® 400 exhibits processing aptitudes strongly improved compared to conventional steel W1.2711 or equivalent, heat treated to same hardness. This improvement mainly results from a new chemical balance. SUPERPLAST® 400, delivered at 350 to 380 HB, has excellent weldability, a better micro structural homogeneity and a much better machinability than conventional grades heat treated to the same level or even lower hardness.

All injection molds demanding high mechanical properties: long series; high injection series; injection of reinforced plastics (glass fibers); wear problems; compression molds

Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.